Page 161 - My FlipBook
P. 161


SILICATE IN THE MAKING OP A FILLING 157

to hasten the chemical action and better results -will be secured.
With most of the silicate fillings, the body temperature is suf-
ficient with others the best result can only be obtained by keeping
;























Fig. 95.—Taking the first portion of the powder which should be about half of the entire
amount needed.
























Fig. 96.—Incorporating the first portion of the powder.

the filling for a short time bathed in melted parafiine. The mix-
ing slab should be at as low a temperature as possible and should not
produce discomfiture to the patient. A temperature of 60 degrees
   156   157   158   159   160   161   162   163   164   165   166